Specification and qualification of welding procedures for metallic materials - Qualification based on previous welding experience (ISO 15611:2003)

This European Standard gives the necessary information to explain the requirements referenced in EN ISO 15607 about the qualification of welding procedures based on previous welding experience. In addition it gives the range of qualification and the validity. The use of this European Standard may be restricted by an application standard or a specification.
ΚΩΔΙΚΟΣ ΠΡΟΪΟΝΤΟΣ: CYS EN ISO 15611:2003
€26.00
This European Standard gives the necessary information to explain the requirements referenced in EN ISO 15607 about the qualification of welding procedures based on previous welding experience. In addition it gives the range of qualification and the validity. The use of this European Standard may be restricted by an application standard or a specification.